Effect of heat treatment on the microstructure characteristics and microhardness of a novel γ′ nickel-based superalloy by laser powder bed fusion

Xu, Jinghao, 1992- (författare)
Linköpings universitet,Konstruktionsmaterial,Tekniska fakulteten
Schulz, Fiona, 1990 (författare)
Chalmers tekniska högskola,Chalmers University of Technology,Div of Materials and Manufacture, Dept of Industrial and Mateials Science, Chalmers, Gothenburg
Peng, Ru Lin, 1960- (författare)
Linköpings universitet,Konstruktionsmaterial,Tekniska fakulteten
visa fler...
Hryha, Eduard, 1980 (författare)
Chalmers tekniska högskola,Chalmers University of Technology,Div of Materials and Manufacture, Dept of Industrial and Mateials Science, Chalmers, Gothenburg
Moverare, Johan, 1973- (författare)
Linköpings universitet,Konstruktionsmaterial,Tekniska fakulteten
visa färre...
 (creator_code:org_t)
Elsevier BV, 2021
2021
Engelska.
Ingår i: Results in Materials. - : Elsevier BV. - 2590-048X. ; 12
  • Tidskriftsartikel (refereegranskat)
Abstract Ämnesord
Stäng  
  • The fabrication of gamma prime (γ′) strengthened nickel-based superalloys by additive manufacturing (AM) techniques is of huge interest from the industrial and research community owing to their excellent high-temperature properties. The effect of post-AM-processing heat treatment on the microstructural characteristics and microhardness response of a laser powder bed fused (LPBF) γ′ strengthened nickel-based superalloy, MAD542, is systematically investigated. Post-processing heat treatment shows the significant importance of tailoring the γ′ morphology. With insufficient solutioning duration time, coarse γ′ formed in the interdendritic region heterogeneously, due to the lack of chemical composition homogenization. The cooling rate from the super-solvus solutioning plays an important role in controlling the γ′ size and morphology. Spherical γ′ is formed during the air cooling while irregularly shaped γ′ formed during the furnace cooling. The following aging heat treatment further tunes the γ′ morphology and γ channel width. After two-step aging, cuboidal γ′ is developed in the air-cooled sample, while in contrast, bi-modally distributed γ′ is developed in the furnace cooled sample with fine spherical γ′ embedded in the wide γ channel between coarse irregular shaped secondary γ′. More than 90% of the grains recrystallized during solutioning treatment at the super-solvus temperature for 30 min. The rapid recrystallization kinetics are attributed to the formation of annealing twins which significantly reduced the stored energy. Microhardness responses from different heat-treated conditions were examined.

Ämnesord

TEKNIK OCH TEKNOLOGIER  -- Maskinteknik -- Energiteknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Mechanical Engineering -- Energy Engineering (hsv//eng)
TEKNIK OCH TEKNOLOGIER  -- Annan teknik -- Livsmedelsteknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Other Engineering and Technologies -- Food Engineering (hsv//eng)
TEKNIK OCH TEKNOLOGIER  -- Materialteknik -- Metallurgi och metalliska material (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Materials Engineering -- Metallurgy and Metallic Materials (hsv//eng)
TEKNIK OCH TEKNOLOGIER  -- Materialteknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Materials Engineering (hsv//eng)

Nyckelord

Recrystallization
LPBF
Nickel-based superalloy
Gamma prime γ′
Heat treatment

Publikations- och innehållstyp

art (ämneskategori)
ref (ämneskategori)

Hitta via bibliotek

Till lärosätets databas

Sök utanför SwePub

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Stäng

Kopiera och spara länken för att återkomma till aktuell vy