Sökning: id:"swepub:oai:research.chalmers.se:2586a667-1e6c-48b5-bf64-36e9c45cf9ca" > Fatigue Isotropy in...

Fatigue Isotropy in Cross-Rolled, Hardened Isotropic-Quality Steel

Temmel, Cornelius, 1973 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
Karlsson, Birger, 1941 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
Ingesten, Nils-Gunnar (författare)
 (creator_code:org_t)
2008-03-12
2008
Engelska.
Ingår i: Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science. - : Springer Science and Business Media LLC. - 1073-5623. ; 39A:5, s. 1132-1144
  • Tidskriftsartikel (refereegranskat)
Abstract Ämnesord
Stäng  
  • Deformation and forging operations often introduce microstructural orientation and, therewith, mechanical anisotropy to steel. Flattened manganese sulfide inclusions are held responsible for a great part of fatigue anisotropy. Isotropic-quality (IQ) steel maintains the mechanical isotropy of the material, even after a deformation operation. Isotropic material generally contains little S and, therewith, few manganese sulfides. Further, the IQ steels used in this investigation were Ca treated. The Ca treatment improves the shape stability of the sulfides, even during a hot-working deformation. Two commercial materials were compared for their fatigue response, a standard medium-carbon steel with 0.04 wt pct S and a low-sulfur variant that underwent IQ treatment. The two batches were cross-rolled to plates with a deformation ratio of 4.5, leading to in-plane isotropy. Tension-compression fatigue testing was performed in longitudinal and short transversal directions relative to the rolling plane. The results showed strong anisotropy of the fatigue behavior for the standard material. The performance in the short transverse direction, with the principal stress perpendicular to the flattened inclusions, was inferior. The IQ material with nearly spherical inclusions was almost perfectly isotropic, with only slightly worse fatigue response in the short transverse direction. © The Minerals, Metals & Materials Society and ASM International 2008.

Ämnesord

TEKNIK OCH TEKNOLOGIER  -- Materialteknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Materials Engineering (hsv//eng)

Publikations- och innehållstyp

art (ämneskategori)
ref (ämneskategori)

Hitta via bibliotek

Till lärosätets databas

Sök utanför SwePub

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Stäng

Kopiera och spara länken för att återkomma till aktuell vy