Defects and the thermal conductivity of YBa2Cu3O7-d and YBa2Cu4O8
- 1993
-
Ingår i: Journal of Alloys and Compounds, volume 195. - : Elsevier Sequoia S.A.. - 0 444 81529 5 ; , s. 655-658
-
Konferensbidrag (refereegranskat)abstract
- We present below the first measured data for the thermal diffusivity and the thermal conductivity, λ, of dense, sintered ceramic YBa2Cu4O8 (1-2-4) as a function of temperature T between 40 and 310 K. At 300 K, λ is 6.3 Wm−1K−1, increasing with decreasing T to about 9.5 Wm−1K−1 near Tc. This T dependence is much stronger than in YBa2Cu3O7−δ (1-2-3). Only a very small enhancement is observed in λ below Tc. As in 1-2-3, λ is mainly limited by phonon scattering by defects.
|
|