An in vitro study of blood compatibility of vascular grafts made of bacterial cellulose in comparison with conventionally-used graft materials

Fink, Helen, 1978 (författare)
Gothenburg University,Göteborgs universitet,Institutionen för kliniska vetenskaper, Avdelningen för kirurgi,Institute of Clinical Sciences, Department of Surgery
Hong, Jaan (författare)
Uppsala universitet,Klinisk immunologi,Forskargrupp Bo Nilsson,Akademiska Sjukhuset
Drotz, Kristoffer, 1984 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
visa fler...
Risberg, Bo, 1941 (författare)
Gothenburg University,Göteborgs universitet,Institutionen för kliniska vetenskaper, Avdelningen för kirurgi,Institute of Clinical Sciences, Department of Surgery
Sanchez, Javier (författare)
Uppsala universitet,Klinisk immunologi,Akademiska Sjukhuset
Sellborn, Anders, 1966 (författare)
Gothenburg University,Göteborgs universitet,Institutionen för kliniska vetenskaper, Avdelningen för kirurgi,Institute of Clinical Sciences, Department of Surgery
visa färre...
 (creator_code:org_t)
2011-02-09
2011
Engelska.
Ingår i: Journal of Biomedical Materials Research - Part A. - : Wiley. - 1549-3296 .- 1552-4965. ; 97A:1, s. 52-58
  • Tidskriftsartikel (refereegranskat)
Abstract Ämnesord
Stäng  
  • In this study we analyzed the blood compatibility of bacterial cellulose (BC) as a new biosynthetic material for use as a vascular graft. As reference materials we used expanded polytetrafluoroethylene (ePTFE) and poly(ethylene terephthalate) (PET) vascular grafts. These materials are in clinical use today. Tubes with inner diameters of both 4 (not PET) and 6 mm were tested. Heparin-coated PVC tubes (hepPVC) were used as a negative control. Platelet consumption and thrombin-antithrombin complex (TAT) were used as parameters of coagulation and for complement activation, sC3a and sC5b-9 were used. The investigated parameters were measured after 1-h exposure to freshly drawn human blood supplemented with a low dose of heparin in a Chandler loop system. The results showed that BC exhibits no significant difference in platelet consumption, as compared with PET 16 mm), ePTFE and hepPVC. The PET material consumed more platelets than any of the other materials. The TAT generation for 4 mm tubes was not significantly different between BC and the other materials. For 6 mm tubes, however, differences were observed between hepPVC and PET (p < 0.0001); BC and hepPVC (p = 0.0016); ePTFE and PET (p < 0.0001); BC and ePTFE (p = 0.0029); BC and PET (p = 0.0141). Surprisingly, considering the low platelet consumption, the complement activation parameters (sC3a and sC5b-9) were much higher for BC, as compared with the other materials for both 4 and 6 mm tubes.

Ämnesord

MEDICIN OCH HÄLSOVETENSKAP  -- Klinisk medicin -- Kirurgi (hsv//swe)
MEDICAL AND HEALTH SCIENCES  -- Clinical Medicine -- Surgery (hsv//eng)

Nyckelord

bacterial cellulose
blood compatibility
coagulation
complement activation
Chandler loop
PET
ePTFE
MEDICINE
MEDICIN

Publikations- och innehållstyp

ref (ämneskategori)
art (ämneskategori)

Hitta via bibliotek

Till lärosätets databas

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Stäng

Kopiera och spara länken för att återkomma till aktuell vy