Sökning: onr:"swepub:oai:research.chalmers.se:1944ea56-b92a-40ae-a93a-eddc32be6658" >
Characterization of...
Characterization of Pt/γ-Al2O3 catalysts deactivated by hexamethyldisiloxane
-
- Arnby, Karl, 1974 (författare)
- Chalmers tekniska högskola,Chalmers University of Technology
-
- Rahmani, Mohammad (författare)
- Amirkabir University of Technology
-
- Sanati, Mehri (författare)
- Lund University,Lunds universitet,Ergonomi och aerosolteknologi,Institutionen för designvetenskaper,Institutioner vid LTH,Lunds Tekniska Högskola,Ergonomics and Aerosol Technology,Department of Design Sciences,Departments at LTH,Faculty of Engineering, LTH
-
visa fler...
-
- Cruise, Neil (författare)
- Perstorp Formox
-
- Amberntsson Carlsson, Annika (författare)
- Perstorp Formox
-
- Skoglundh, Magnus, 1965 (författare)
- Chalmers tekniska högskola,Chalmers University of Technology
-
visa färre...
-
(creator_code:org_t)
- Elsevier BV, 2004
- 2004
- Engelska.
-
Ingår i: Applied Catalysis B: Environmental. - : Elsevier BV. - 0926-3373 .- 1873-3883. ; 54:1, s. 1-7
- Relaterad länk:
-
http://dx.doi.org/10...
-
visa fler...
-
https://research.cha...
-
https://doi.org/10.1...
-
https://lup.lub.lu.s...
-
visa färre...
Abstract
Ämnesord
Stäng
- The deactivation of alumina supported platinum and iron catalysts by hexamethyldisiloxane (HMDS) exposure has been investigated. Three catalysts (Pt/Al2O3, Fe/Al2O3 and Fe/Pt/Al2O3) were prepared and the influence of short- and long-term deactivation on the activity for oxidation of ethyl acetate was studied. The catalysts were characterized using BET, ICP-AES, XPS, SEM and CO chemisorption. The deactivation was found to proceed by deposition of silicon-species in form of silicate (SixOy) that block the active sites on the surface of the catalysts. The silicon seems to rather attach to platinum and iron sites than to the alumina surface. The Pt/Al2O3 catalyst was moderately deactivated by HMDS even though the silicate was blocking almost the entire platinum surface. Adding iron to the catalyst increased the tolerance towards HMDS as fewer Pt sites were blocked for the Fe/Pt/Al2O3 sample. The deactivation of the two platinum containing samples was reversible since the silicate could partly be removed from the Pt sites by regeneration whereby most of the activity was restored. However, for the Fe/Al2O3 sample the deactivation was more severe and irreversible.
Ämnesord
- TEKNIK OCH TEKNOLOGIER -- Kemiteknik (hsv//swe)
- ENGINEERING AND TECHNOLOGY -- Chemical Engineering (hsv//eng)
- NATURVETENSKAP -- Geovetenskap och miljövetenskap -- Miljövetenskap (hsv//swe)
- NATURAL SCIENCES -- Earth and Related Environmental Sciences -- Environmental Sciences (hsv//eng)
- TEKNIK OCH TEKNOLOGIER -- Maskinteknik -- Produktionsteknik, arbetsvetenskap och ergonomi (hsv//swe)
- ENGINEERING AND TECHNOLOGY -- Mechanical Engineering -- Production Engineering, Human Work Science and Ergonomics (hsv//eng)
Nyckelord
- Platinum
- Alumina
- Iron
- Silicon
- Ethyl acetate oxidation
- Hexamethyldisiloxane
- Deactivation
- silicon
- deactivation
- hexamethyldisiloxane
- ethyl acetate oxidation
- platinum
- iron
- alumina
Publikations- och innehållstyp
- art (ämneskategori)
- ref (ämneskategori)
Hitta via bibliotek
Till lärosätets databas