1.
  • Huang, Wen, et al. (author)
  • Concentration dependence of hydrogen diffusion in clamped vanadium (001) films
  • 2017
  • In: Journal of Physics. - 0953-8984 .- 1361-648X. ; 29:4
  • Journal article (peer-reviewed)abstract
    • The chemical diffusion coefficient of hydrogen in a 50 nm thin film of vanadium (0 0 1) is measured as a function of concentration and temperature, well above the known phase boundaries. Arrhenius analysis of the tracer diffusion constants reveal large changes in the activation energy with concentration: from 0.10 at 0.05 in II V-1 to 0.5 eV at 0.2 in II V-1. The results are consistent with a change from tetrahedral to octahedral site occupancy, in that concentration range. The change in site occupancy is argued to be caused by the uniaxial expansion of the film originating from the combined hydrogen induced expansion and the clamping of the film to the substrate.
  •  
2.
  • Asano, Kohta, et al. (author)
  • Destabilization of Mg Hydride by Self-Organized Nanoclusters in the Immiscible Mg-Ti System
  • 2015
  • In: The Journal of Physical Chemistry C. - : American Chemical Society (ACS). - 1932-7447 .- 1932-7455. ; 119:22, s. 12157-12164
  • Journal article (peer-reviewed)abstract
    • Mg is an attractive hydrogen storage material not only because of its high gravimetric and volumetric hydrogen capacities but also because of it low material costs. However, the hydride of MgH2 is too stable to release hydrogen under moderate conditions. We demonstrate that the formation of nanometer-sized clusters of Mg reduces the stability of MgH2 by the interface energy effect in the immiscible Mg-Ti system. Ti-rich MgxTi1-x (x < 0.5) thin films deposited by magnetron sputtering have a hexagonal close packed (HCP) structure, which forms a face-centered cubic (FCC) hydride phase upon hydrogenation. Positron Doppler broadening depth profiling demonstrates that after hydrogenation, nanometer-sized MgH2 clusters are formed which are coherently embedded in an FCC TiH2 matrix. The P (pressure)-T (optical transmission) isotherms measured by hydrogenography show that these MgH2 clusters are destabilized. This indicates that the formation of nanometer-sized Mg allows for the development of a lightweight and cheap hydrogen storage material with a lower desorption temperature.
  •  
Skapa referenser, mejla, bekava och länka
  • Result 1-2 of 2

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Close

Copy and save the link in order to return to this view