Search: onr:"swepub:oai:DiVA.org:kth-156127" > Hydrothermal ageing...
Fältnamn | Indikatorer | Metadata |
---|---|---|
000 | 05286naa a2200517 4500 | |
001 | oai:DiVA.org:kth-156127 | |
003 | SwePub | |
008 | 141121s2014 | |||||||||||000 ||eng| | |
009 | oai:DiVA.org:his-16609 | |
024 | 7 | a https://urn.kb.se/resolve?urn=urn:nbn:se:kth:diva-1561272 URI |
024 | 7 | a https://doi.org/10.1016/j.polymdegradstab.2014.06.0102 DOI |
024 | 7 | a https://urn.kb.se/resolve?urn=urn:nbn:se:his:diva-166092 URI |
040 | a (SwePub)kthd (SwePub)his | |
041 | a engb eng | |
042 | 9 SwePub | |
072 | 7 | a ref2 swepub-contenttype |
072 | 7 | a art2 swepub-publicationtype |
100 | 1 | a Gil-Castell, O.u Instituto de Tecnología de Materiales (ITM), Universitat Politecnica de Valencia (UPV), Valencia, Spain4 aut |
245 | 1 0 | a Hydrothermal ageing of polylactide/sisal biocomposites. Studies of water absorption behaviour and Physico-Chemical performance |
264 | 1 | b Elsevier BV,c 2014 |
338 | a print2 rdacarrier | |
500 | a QC 20141217 | |
520 | a An accelerated hydrothermal degrading test was designed in order to analyse the synergic effect of water and temperature on PLA/sisal biocomposites with and without coupling agent. As well, the physicochemical properties of biocomposites were monitored along the hydrothermal test by means of Scanning Electron Microscopy, Size Exclusion Chromatography and Differential Scanning Calorimetry. The addition of fibre induced higher water absorption capability and promoted physical degradation, as observed in the surface topography. During the processing of biocomposites and throughout the hydrothermal ageing, a reduction of molecular weight due to chain scission was found. As a consequence, a faster formation of crystalline domains in the PIA matrix occurred the higher the amount of fibre was, which acted as a nucleating agent. Higher crystallinity was considered as a barrier against the advance of penetrant and a reduction in the diffusion coefficient was shown. The addition of coupling agent presented a different influence depending on the composition, showing an inflection point around 20% of sisal fibre. | |
650 | 7 | a NATURVETENSKAPx Kemix Polymerkemi0 (SwePub)104062 hsv//swe |
650 | 7 | a NATURAL SCIENCESx Chemical Sciencesx Polymer Chemistry0 (SwePub)104062 hsv//eng |
650 | 7 | a TEKNIK OCH TEKNOLOGIERx Kemiteknikx Polymerteknologi0 (SwePub)204032 hsv//swe |
650 | 7 | a ENGINEERING AND TECHNOLOGYx Chemical Engineeringx Polymer Technologies0 (SwePub)204032 hsv//eng |
653 | a Biocomposites | |
653 | a Polylactide (PLA) | |
653 | a Natural fibres | |
653 | a Sisal | |
653 | a Hydrothermal degradation | |
653 | a Water absorption | |
700 | 1 | a Badia, J. D.u Instituto de Tecnología de Materiales (ITM), Universitat Politecnica de Valencia (UPV), Valencia, Spain / Departament d'Enginyeria Química, Escola Tecnica Superior d'Enginyeria, Universitat de Valencia, Burjassot, Spain4 aut |
700 | 1 | a Kittikorn, Thorsaku KTH,Fiber- och polymerteknologi,Department of Fibre and Polymer Technology, School of Chemical Science and Engineering, KTH Royal Institute of Technology, Stockholm, Sweden / Department of Materials Science and Technology, Faculty of Science, Prince of Songkla University Songkhla, Thailand4 aut0 (Swepub:kth)u1ta2ri4 |
700 | 1 | a Strömberg, Emmau KTH,Fiber- och polymerteknologi,Department of Fibre and Polymer Technology, School of Chemical Science and Engineering, KTH Royal Institute of Technology, Stockholm, Sweden4 aut0 (Swepub:kth)u1hnbchc |
700 | 1 | a Martinez-Felipe, A.u Instituto de Tecnología de Materiales (ITM), Universitat Politecnica de Valencia (UPV), Valencia, Spain / Departamento de Química Organica, Facultad de Ciencias, Instituto de Ciencia de Materiales de Aragon (ICMA), Universidad de Zaragoza-CSIC, Spain4 aut |
700 | 1 | a Ek, Monicau KTH,Fiber- och polymerteknologi,Department of Fibre and Polymer Technology, School of Chemical Science and Engineering, KTH Royal Institute of Technology, Stockholm, Sweden4 aut0 (Swepub:kth)u1hylg9m |
700 | 1 | a Karlsson, Sigbrittu Högskolan i Skövde,KTH,Fiber- och polymerteknologi,University of Skövde, Sweden,Department of Fibre and Polymer Technology, School of Chemical Science and Engineering, KTH Royal Institute of Technology, Stockholm, Sweden4 aut0 (Swepub:his)karb |
700 | 1 | a Ribes-Greus, A.u Instituto de Tecnología de Materiales (ITM), Universitat Politecnica de Valencia (UPV), Spain4 aut |
710 | 2 | a Instituto de Tecnología de Materiales (ITM), Universitat Politecnica de Valencia (UPV), Valencia, Spainb Instituto de Tecnología de Materiales (ITM), Universitat Politecnica de Valencia (UPV), Valencia, Spain / Departament d'Enginyeria Química, Escola Tecnica Superior d'Enginyeria, Universitat de Valencia, Burjassot, Spain4 org |
773 | 0 | t Polymer degradation and stabilityd : Elsevier BVg 108, s. 212-222q 108<212-222x 0141-3910x 1873-2321 |
856 | 4 | u https://riunet.upv.es/bitstream/10251/62790/1/PDST2014.%20OGilCastell_JDBadia_TKittikorn_EStromberg_AMartinezFelipe_MEk_SKarlsson_ARibesGreus.pdf |
856 | 4 8 | u https://urn.kb.se/resolve?urn=urn:nbn:se:kth:diva-156127 |
856 | 4 8 | u https://doi.org/10.1016/j.polymdegradstab.2014.06.010 |
856 | 4 8 | u https://urn.kb.se/resolve?urn=urn:nbn:se:his:diva-16609 |
Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.
Copy and save the link in order to return to this view