SwePub
Sök i LIBRIS databas

  Extended search

onr:"swepub:oai:research.chalmers.se:08bbbbb1-8a0f-4df3-8662-c8cc7d401a8f"
 

Search: onr:"swepub:oai:research.chalmers.se:08bbbbb1-8a0f-4df3-8662-c8cc7d401a8f" > A Fullerene Alloy B...

  • 1 of 1
  • Previous record
  • Next record
  •    To hitlist

A Fullerene Alloy Based Photovoltaic Blend with a Glass Transition Temperature above 200 °C

Diaz de Zerio Mendaza, Amaia, 1986 (author)
Chalmers tekniska högskola,Chalmers University of Technology
Melianas, A. (author)
Linköpings universitet,Linköping University
Nugroho, Ferry, 1986 (author)
Chalmers tekniska högskola,Chalmers University of Technology
show more...
Bäcke, Olof, 1984 (author)
Chalmers tekniska högskola,Chalmers University of Technology
Olsson, Eva, 1960 (author)
Chalmers tekniska högskola,Chalmers University of Technology
Langhammer, Christoph, 1978 (author)
Chalmers tekniska högskola,Chalmers University of Technology
Inganäs, Olle (author)
Linköpings universitet,Linköping University
Müller, Christian, 1980 (author)
Chalmers tekniska högskola,Chalmers University of Technology
show less...
 (creator_code:org_t)
2017
2017
English.
In: Journal of Materials Chemistry A. - 2050-7488 .- 2050-7496. ; 5:8, s. 4156-4162
  • Journal article (peer-reviewed)
Abstract Subject headings
Close  
  • Organic solar cells with a high degree of thermal stability require bulk-heterojunction blends that feature a high glass transition, which must occur considerably above the temperatures encountered during device fabrication and operation. Here, we demonstrate for the first time a polymer : fullerene blend with a glass transition temperature above 200 °C, which we determine by plasmonic nanospectroscopy. We achieve this strong tendency for glass formation through the use of an alloy of neat, unsubstituted C60 and C70, which we combine with the fluorothieno-benzodithiophene copolymer PTB7. A stable photovoltaic performance of PTB7 : C60 : C70 ternary blends is preserved despite annealing the active layer at up to 180 °C, which coincides with the onset of the glass transition. Rapid deterioration of the power conversion efficiency from initially above 5% only occurs upon exceeding the glass transition temperature of 224 °C of the ternary blend.

Subject headings

NATURVETENSKAP  -- Kemi -- Polymerkemi (hsv//swe)
NATURAL SCIENCES  -- Chemical Sciences -- Polymer Chemistry (hsv//eng)
NATURVETENSKAP  -- Kemi -- Materialkemi (hsv//swe)
NATURAL SCIENCES  -- Chemical Sciences -- Materials Chemistry (hsv//eng)
NATURVETENSKAP  -- Fysik -- Annan fysik (hsv//swe)
NATURAL SCIENCES  -- Physical Sciences -- Other Physics Topics (hsv//eng)

Publication and Content Type

art (subject category)
ref (subject category)

Find in a library

To the university's database

  • 1 of 1
  • Previous record
  • Next record
  •    To hitlist

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Close

Copy and save the link in order to return to this view