A New High-Temperature Durable Absorber Material Solution through a Spinel-Type High Solar Absorptivity Coating on Ti2AlC MAX Phase Material

Wang, Wujun, 1984- (författare)
KTH,Kraft- och värmeteknologi
Fei, Ye, 1979- (författare)
KTH,Material- och nanofysik
Mu, Wangzhong, Dr. 1985- (författare)
KTH,Strukturer
visa fler...
Dutta, Joydeep, Professor, 1964- (författare)
KTH,Material- och nanofysik,Dept Appl Phys, S-11419 Stockholm, Sweden.;King Abdulaziz Univ, Ctr Nanotechnol, Jeddah 21589, Saudi Arabia.
Laumert, Björn (författare)
KTH,Kraft- och värmeteknologi
visa färre...
 (creator_code:org_t)
2021-09-08
2021
Engelska.
Ingår i: ACS Applied Materials and Interfaces. - : American Chemical Society (ACS). - 1944-8244 .- 1944-8252. ; 13:37, s. 45008-45017
  • Tidskriftsartikel (refereegranskat)
Abstract Ämnesord
Stäng  
  • Enhancing the operating temperature of concentrating solar power systems is a promising way to obtain higher system efficiency and thus enhance their competitiveness. One major barrier is the unavailability of suitable solar absorber materials for operation at higher temperatures. In this work, we report on a new high-temperature absorber material by combining Ti2AlC MAX phase material and iron-cobalt-chromite spinel coating/paint. This durable material solution exhibits excellent performance, passing the thermal stability test in an open-air environment at a temperature of 1250 degrees C for 400 h and at 1300 degrees C for 200 h. The results show that the black spinel coating can offer a stable high solar absorptivity in the range of 0.877-0.894 throughout the 600 h test under high temperatures. These solar absorptivity values are even 1.6-3.3% higher than that for the sintered SiC ceramic that is a widely used solar absorber material. Divergence of solar absorptivity during these relatively long testing periods is less than 1.1%, indicating remarkable stability of the absorber material. Furthermore, considering the simple application process of the coating/painting utilizing a brush followed by curing at relatively low temperatures (room temperature, 95 and 260 degrees C in sequence), this absorber material shows the potential for large-scale, high-temperature solar thermal applications.

Ämnesord

TEKNIK OCH TEKNOLOGIER  -- Maskinteknik -- Energiteknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Mechanical Engineering -- Energy Engineering (hsv//eng)

Nyckelord

solar receiver
MAX phase
iron-cobalt-chromite spinel coating
spectral hemispherical absorptivity
concentrating solar power
thermal stability

Publikations- och innehållstyp

ref (ämneskategori)
art (ämneskategori)

Hitta via bibliotek

Till lärosätets databas

Sök utanför SwePub

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Stäng

Kopiera och spara länken för att återkomma till aktuell vy