- Wani, M. F., et al.
(författare)
-
Friction and wear behaviour of hot pressed SiAlON‑steel ball tribopair under reciprocating sliding conditions
- 1993
-
Ingår i: American Ceramic Society Bulletin. - 0002-7812 .- 1945-2705. ; 7:9, s. 82-87
-
Tidskriftsartikel (refereegranskat)abstract
- Friction and wear characteristics of SiAlON (Si(6-x)Al(x)O(x)N(8-x) where x = 0.5, 1.0, and 2.0), pressure sintered with the composition shifted toward the oxygen corner, were studied using a steel ball bearing as the second member of a tribopair under reciprocating sliding conditions. Sliding distance, velocity, and load were the test variables.
|
|
10. |
- Wani, M. F., et al.
(författare)
-
Friction and wear of HPSN bearing materials
- 1997
-
Ingår i: American Ceramic Society Bulletin. - 0002-7812 .- 1945-2705. ; 76:8, s. 65-69
-
Tidskriftsartikel (refereegranskat)abstract
- Paper presents data on wear and friction of hot-pressed silicon nitride (HPSN) and its composites in contact with ball-bearing steel. The coefficient of friction under unlubricated sliding conditions was 0.45, and it did not change with load under lubricated conditions. The wear coefficient was the least for HPSN sintered with liquid in system containing yttria. HPSN containing 15 % of TiC showed the best wear resistance compared to HPSN with other concentrations of TiC or BN. No adhesive wear was detected.
|
|