Sökning: onr:"swepub:oai:lup.lub.lu.se:295c9862-4a92-4051-9e50-42a0ea7b45b5" >
Structural, optical...
Structural, optical, and luminescence properties of ZnO:Ga optical scintillation ceramic
-
- Gorokhova, E. I. (författare)
- Vavilov State Optical Institute
-
- Eron’Ko, S. B. (författare)
- Vavilov State Optical Institute
-
- Oreshchenko, E. A. (författare)
- Vavilov State Optical Institute
-
visa fler...
-
- Sandulenko, A. V. (författare)
- Vavilov State Optical Institute
-
- Rodnyi, P. A. (författare)
- St. Petersburg State Polytechnical University
-
- Chernenko, K. A. (författare)
- Lund University,Lunds universitet,MAX IV-laboratoriet,MAX IV Laboratory,St. Petersburg State Polytechnical University
-
- Venevtsev, I. D. (författare)
- St. Petersburg State Polytechnical University
-
- Kul’Kov, A. M. (författare)
- Saint Petersburg State University
-
- Muktepavela, Faina (författare)
- University of Latvia
-
- Boutachkov, Plamen (författare)
- GSI Helmholtz Centre for Heavy Ion Research
-
visa färre...
-
Vavilov State Optical Institute St Petersburg State Polytechnical University (creator_code:org_t)
- 2018
- 2018
- Engelska 9 s.
-
Ingår i: Journal of Optical Technology (A Translation of Opticheskii Zhurnal). - 1070-9762. ; 85:11, s. 729-737
- Relaterad länk:
-
http://dx.doi.org/10...
-
visa fler...
-
https://lup.lub.lu.s...
-
https://doi.org/10.1...
-
visa färre...
Abstract
Ämnesord
Stäng
- This paper discusses the characteristics of ZnO and ZnO:Ga ceramics fabricated by uniaxial hot pressing. The short-wavelength transmission limit of zinc oxide ceramics is in the 370-nm region; the long-wavelength limit is determined by the free-charge-carrier concentration and lies in the interval from 5 to 9 μm. The total transmittance of such ceramics in the visible and near-IR regions is about 70% when the sample is 0.5 mm thick. The luminescence spectrum is represented by a broad emission band with maximum at 580 nm, having a defect nature. The introduction of 0.03–0.1 mass % gallium into the zinc oxide structure inhibits grain growth and increases the free-charge-carrier concentration to 3.44 × 1019 cm−3. As the gallium concentration increases in the range 0.05–0.1 mass % in a ceramic of composition ZnO:Ga, the defect luminescence band is suppressed and a characteristic exciton luminescence is formed with a maximum corresponding to 389 nm and a damping time constant of 1.1 ns.
Ämnesord
- NATURVETENSKAP -- Fysik -- Den kondenserade materiens fysik (hsv//swe)
- NATURAL SCIENCES -- Physical Sciences -- Condensed Matter Physics (hsv//eng)
Publikations- och innehållstyp
- art (ämneskategori)
- ref (ämneskategori)
Hitta via bibliotek
Till lärosätets databas
- Av författaren/redakt...
-
Gorokhova, E. I.
-
Eron’Ko, S. B.
-
Oreshchenko, E. ...
-
Sandulenko, A. V ...
-
Rodnyi, P. A.
-
Chernenko, K. A.
-
visa fler...
-
Venevtsev, I. D.
-
Kul’Kov, A. M.
-
Muktepavela, Fai ...
-
Boutachkov, Plam ...
-
visa färre...
- Om ämnet
-
- NATURVETENSKAP
-
NATURVETENSKAP
-
och Fysik
-
och Den kondenserade ...
- Artiklar i publikationen
-
Journal of Optic ...
- Av lärosätet
-
Lunds universitet