NH3-SCR activity of H-BEA and Fe-BEA after potassium exposure

Shwan, Soran, 1984 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
Jansson, Jonas, 1973 (författare)
Volvo Group
Olsson, Louise, 1974 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
visa fler...
Skoglundh, Magnus, 1965 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
visa färre...
 (creator_code:org_t)
2015-08-11
2015
Engelska.
Ingår i: Topics in Catalysis. - : Springer Science and Business Media LLC. - 1572-9028 .- 1022-5528. ; 58:14-17, s. 1012-1018
  • Tidskriftsartikel (refereegranskat)
Abstract Ämnesord
Stäng  
  • A previous developed multisite microkinetic model for hydrothermally deactivated H-BEA and Fe-BEA catalyst used for NH3-SCR applications has been applied and validated using potassium exposed H-BEA and Fe-BEA samples. The catalysts have been exposed to evaporated aqueous solution of potassium (10 ppm KNO3) in a flow-reactor for 14-48 h. The results for the H-BEA samples show an increase in NH3-SCR activity after 48 h of potassium exposure. This is correlated to an increase in NOX storage capacity, indicating that potassium forms new NOX storage sites participating in the SCR reaction. However, the Fe-BEA samples show different results. The SCR activity for the Fe-BEA catalyst decreases significantly after 14 h of exposure to potassium and after longer exposure time the activity slightly increases again compared to the sample exposed to potassium for 14 h. When applying the kinetic model to the flow-reactor measurements the model is able to predict the changes in SCR activity well when changing the site density of the active sites. In overall, combining the experimental results with the simulation indicates that exposure to potassium initially chemically blocks the active iron species which decrease with exposure time. Longer time of exposure to potassium indicates that the iron species are exchanged and lost due to formation of new potassium sites in the zeolite resulting in an overall lower SCR activity compared to a fresh Fe-BEA sample.

Ämnesord

NATURVETENSKAP  -- Kemi -- Fysikalisk kemi (hsv//swe)
NATURAL SCIENCES  -- Chemical Sciences -- Physical Chemistry (hsv//eng)
TEKNIK OCH TEKNOLOGIER  -- Kemiteknik -- Kemiska processer (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Chemical Engineering -- Chemical Process Engineering (hsv//eng)
TEKNIK OCH TEKNOLOGIER  -- Kemiteknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Chemical Engineering (hsv//eng)

Nyckelord

Kinetic modeling
Poisoning
Fe-BEA
Deactivation
NH3-SCR
Potassium

Publikations- och innehållstyp

art (ämneskategori)
ref (ämneskategori)

Hitta via bibliotek

Till lärosätets databas

Hitta mer i SwePub

Av författaren/redakt...
Shwan, Soran, 19 ...
Jansson, Jonas, ...
Olsson, Louise, ...
Skoglundh, Magnu ...
Om ämnet
NATURVETENSKAP
NATURVETENSKAP
och Kemi
och Fysikalisk kemi
TEKNIK OCH TEKNOLOGIER
TEKNIK OCH TEKNO ...
och Kemiteknik
och Kemiska processe ...
TEKNIK OCH TEKNOLOGIER
TEKNIK OCH TEKNO ...
och Kemiteknik
Artiklar i publikationen
Topics in Cataly ...
Av lärosätet
Chalmers tekniska högskola

Sök utanför SwePub

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Stäng

Kopiera och spara länken för att återkomma till aktuell vy