Exploring failure modes of alumina scales on FeCrAl and FeNiCrAl alloys in a nitriding environment
-
- Mortazavi, A. N. (författare)
- Harvard University
-
- Esmaily, Mohsen, 1987 (författare)
- Massachusetts Institute of Technology (MIT)
-
- Geers, Christine, 1982 (författare)
- Chalmers tekniska högskola,Chalmers University of Technology
-
visa fler...
-
- Birbilis, N. (författare)
- Australian National University
-
- Svensson, Jan-Erik, 1965 (författare)
- Chalmers tekniska högskola,Chalmers University of Technology
-
- Halvarsson, Mats, 1965 (författare)
- Chalmers tekniska högskola,Chalmers University of Technology
-
- Chandrasekaran, D. (författare)
- Kanthal AB
-
- Johansson, Lars-Gunnar, 1952 (författare)
- Chalmers tekniska högskola,Chalmers University of Technology
-
visa färre...
-
(creator_code:org_t)
- Elsevier BV, 2020
- 2020
- Engelska.
-
Ingår i: Acta Materialia. - : Elsevier BV. - 1359-6454. ; 201, s. 131-146
- Relaterad länk:
-
https://research.cha... (primary) (free)
-
visa fler...
-
https://doi.org/10.1...
-
https://doi.org/10.1...
-
https://research.cha...
-
https://research.cha...
-
visa färre...
Abstract
Ämnesord
Stäng
- Two high-temperature FeCrAl and FeNiCrAl alloys were exposed in a strongly nitriding environment at 900 °C and the morphology of nitridation was studied. Quasi-in-situ experiments revealed that nitridation started at specific surface sites directly related to the alloy microstructure where the alumina scale was permeable to nitrogen. FeCrAl alloy grains with (112) orientation formed outward-growing alumina scales and were susceptible to nitridation. Outward-growing scales and substrate nitridation was also observed at chromium carbide precipitates in the FeNiCrAl alloy. Both alloys suffered nitridation at reactive element-rich (Y and Zr) inclusions larger than a certain critical size. The latter type of attack is caused by cracks and pores in the scale. The findings open new avenues of research for developing the next generation of high temperature alloys with superior properties.
Ämnesord
- TEKNIK OCH TEKNOLOGIER -- Materialteknik -- Bearbetnings-, yt- och fogningsteknik (hsv//swe)
- ENGINEERING AND TECHNOLOGY -- Materials Engineering -- Manufacturing, Surface and Joining Technology (hsv//eng)
- TEKNIK OCH TEKNOLOGIER -- Materialteknik -- Metallurgi och metalliska material (hsv//swe)
- ENGINEERING AND TECHNOLOGY -- Materials Engineering -- Metallurgy and Metallic Materials (hsv//eng)
- TEKNIK OCH TEKNOLOGIER -- Kemiteknik -- Korrosionsteknik (hsv//swe)
- ENGINEERING AND TECHNOLOGY -- Chemical Engineering -- Corrosion Engineering (hsv//eng)
Nyckelord
- Crystallographic orientation
- Reactive elements
- Alumina scale failure
- High temperature oxidation
- Nitridation