Assessment of the reason for the vitrification of a wall at a hillfort. The example of Broborg in Sweden

Sjöblom, Rolf (author)
Luleå tekniska universitet,Geovetenskap och miljöteknik
Hjärthner-Holdar, Eva (author)
Arkeologerna, Geoarchaeological Laboratory, National Historical Museums (SHMM), Hållnäsgatan 11, SE 752 28 Uppsala, Sweden
Pearce, Carolyn I. (author)
Pacific Northwest National Laboratory, 902 Battelle Blvd, Richland, WA 99352, USA
show more...
Weaver, Jamie L. (author)
National Institute of Standards and Technology, Gaithersburg, MD 20899, USA
Ogenhall, Erik (author)
Arkeologerna, Geoarchaeological Laboratory, National Historical Museums (SHMM), Hållnäsgatan 11, SE 752 28 Uppsala, Sweden; Geoveta AB, Sjöängsvägen 2, 192 72 Sollentuna, Sweden
McCloy, John S. (author)
Washington State University, PO Box 642920, Pullman, WA 99164, USA
Marcial, José (author)
Pacific Northwest National Laboratory, 902 Battelle Blvd, Richland, WA 99352, USA
Vicenzi, Edward P. (author)
Smithsonian Institution, Museum Conservation Institute, 4610 Silver Hill Road, Suitland, MD 20746, USA
Schweiger, Michael J. (author)
Pacific Northwest National Laboratory, 902 Battelle Blvd, Richland, WA 99352, USA
Kruger, Albert A. (author)
US Department of Energy, Office of River Protection, Richland, WA 99352, USA
show less...
 (creator_code:org_t)
Elsevier, 2022
2022
English.
In: Journal of Archaeological Science. - : Elsevier. - 2352-409X .- 2352-4103. ; 43
  • Journal article (peer-reviewed)
Abstract Subject headings
Close  
  • It was discovered around 250 years ago that some of the rock material in the walls of some hillforts had been subjected to such high temperature that it had vitrified. This prompted a debate as to the reason for it that is still going on today: did the vitrification come about as a result of hostile action, by accident, or for the purpose of constructing the fort? The present paper is based on the recognition that hillforts are different, and therefore should be evaluated individually. All identifiable factors of interest should be included, and especially those that might disprove any alternative. Thus, incentives, competence and petrographic aspects were evaluated for the hillfort named Broborg (dated to the Migration Period, in Sweden A.D. 400–550), and it is concluded that the vitrification here came about for the purpose of constructing the fort.

Subject headings

HUMANIORA  -- Historia och arkeologi -- Historia (hsv//swe)
HUMANITIES  -- History and Archaeology -- History (hsv//eng)
TEKNIK OCH TEKNOLOGIER  -- Naturresursteknik -- Annan naturresursteknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Environmental Engineering -- Other Environmental Engineering (hsv//eng)

Keyword

Broborg
Vitrified
Hillfort
Vesicles
Genesis
Construction
Avfallsteknik
Waste Science and Technology

Publication and Content Type

ref (subject category)
art (subject category)

Find in a library

To the university's database

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Close

Copy and save the link in order to return to this view