SwePub
Sök i LIBRIS databas

  Utökad sökning

WFRF:(Heikkinen O.)
 

Sökning: WFRF:(Heikkinen O.) > Accelerated deactiv...

Accelerated deactivation studies of the natural-gas oxidation catalyst-Verifying the role of sulfur and elevated temperature in catalyst aging

Honkanen, M. (författare)
Tammerfors tekniska universitet,Tampere University of Technology
Karkkainen, M. (författare)
Oulun Yliopisto,University of Oulu
Kolli, T. (författare)
Oulun Yliopisto,University of Oulu
visa fler...
Heikkinen, O. (författare)
Aalto-Yliopisto,Aalto University
Viitanen, V. (författare)
Aalto-Yliopisto,Aalto University
Zeng, Lunjie, 1983 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
Jiang, H. (författare)
Aalto-Yliopisto,Aalto University
Kallinen, Kauko (författare)
Huuhtanen, M. (författare)
Oulun Yliopisto,University of Oulu
Keiski, R. L. (författare)
Oulun Yliopisto,University of Oulu
Lahtinen, J. (författare)
Aalto-Yliopisto,Aalto University
Olsson, Eva, 1960 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
Vippola, M. (författare)
Tammerfors tekniska universitet,Tampere University of Technology
visa färre...
 (creator_code:org_t)
Elsevier BV, 2016
2016
Engelska.
Ingår i: Applied Catalysis B: Environmental. - : Elsevier BV. - 0926-3373 .- 1873-3883. ; 182, s. 439-448
  • Tidskriftsartikel (refereegranskat)
Abstract Ämnesord
Stäng  
  • Accelerated deactivation, caused by thermal aging (TA) and/or sulfur + water poisoning (SW), of the PtPd/gamma-Al2O3 natural-gas oxidation catalyst was studied. Thermal aging and poisoning treatments were performed separately and with varied combinations and comprehensive characterization of the catalyst was carried out after each step. The fresh catalyst has small, oxidized PtPd particles (<5 nm) uniformly distributed in the gamma-alumina washcoat. After the SW-treatment, a small amount of bulk aluminum sulfate was observed near the slightly grown noble metal particles. During the thermal aging, gamma-alumina changed to delta-/theta- and alpha-alumina. In addition, total decomposition of oxidized Pt and partly decomposition of oxidized Pd occurred resulting in the formation of the grown noble metal particles with a bimetallic PtPd core and a polycrystalline PdO shell. Also few, small (similar to 5 nm) bimetallic PtPd particles were still detected. In the TA + SW-treated catalyst with grown noble metal particles, a small amount of bulk aluminum sulfate was detected and it was randomly distributed over the noble metal particles and washcoat. The activity in the terms of methane conversion over the TA-, SW-, and SW + TA-treated catalysts was similar but it was decreased compared to the fresh catalyst. The activity of the TA+SW-treated catalyst was drastically decreased compared to the fresh catalyst due to significant morphological changes and aluminum sulfate formation.

Ämnesord

TEKNIK OCH TEKNOLOGIER  -- Annan teknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Other Engineering and Technologies (hsv//eng)
NATURVETENSKAP  -- Fysik -- Annan fysik (hsv//swe)
NATURAL SCIENCES  -- Physical Sciences -- Other Physics Topics (hsv//eng)

Nyckelord

Thermal aging
Sulfur poisoning
Palladium
Deactivation
Platinum

Publikations- och innehållstyp

art (ämneskategori)
ref (ämneskategori)

Hitta via bibliotek

Till lärosätets databas

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Stäng

Kopiera och spara länken för att återkomma till aktuell vy