Oxidation of UN/U 2 N 3 -UO 2 composites: an evaluation of UO 2 as an oxidation barrier for the nitride phases

Costa, Diogo Ribeiro (författare)
KTH,Kärnenergiteknik
Hedberg, Marcus, 1987 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
Middleburgh, Simon C. (författare)
Bangor University
visa fler...
Wallenius, Janne, 1968- (författare)
KTH,Kärnenergiteknik
Olsson, Pär (författare)
KTH,Kärnenergiteknik
Lopes, Denise Adorno (författare)
visa färre...
 (creator_code:org_t)
Elsevier BV, 2021
2021
Engelska.
Ingår i: Journal of Nuclear Materials. - : Elsevier BV. - 0022-3115 .- 1873-4820. ; 544
  • Tidskriftsartikel (refereegranskat)
Abstract Ämnesord
Stäng  
  • Composite fuels such as UN-UO2 are being considered to address the lower oxidation resistance of the UN fuel from a safety perspective for use in light water reactors, whilst improving the in-reactor behaviour of the more ubiquitous UO2 fuel. An innovative UN-UO2 accident tolerant fuel has recently been fabricated and studied: UN microspheres embedded in UO2 matrix. In the present study, detailed oxidative thermogravimetric investigations (TGA/DSC) of high-density UN/U2N3-UO2 composite fuels (91-97 %TD), as well as post oxidised microstructures obtained by SEM, are reported and analysed. Triplicate TGA measurements of each specimen were carried out at 5 K/min up to 973 K in a synthetic air atmosphere to assess their oxidation kinetics. The mass variation due to the oxidation reactions (%), the oxidation onset temperatures (OOTs), and the maximum reaction temperatures (MRTs) are also presented and discussed. The results show that all composites have similar post oxidised microstructures with mostly intergranular cracking and spalling. The oxidation resistance of the pellet with initially 10 wt% of UN microspheres is surprisingly better than the UO2 reference. Moreover, there is no significant difference in the OOT (~557 K) and MRT (~615 K) when 30 wt% or 50 wt% of embedded UN microspheres are used. Therefore, the findings in this article demonstrate that the UO2 matrix acts as a barrier to improve the oxidation resistance of the nitride phases at the beginning of life conditions.

Ämnesord

TEKNIK OCH TEKNOLOGIER  -- Kemiteknik -- Kemiska processer (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Chemical Engineering -- Chemical Process Engineering (hsv//eng)
TEKNIK OCH TEKNOLOGIER  -- Kemiteknik -- Annan kemiteknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Chemical Engineering -- Other Chemical Engineering (hsv//eng)
TEKNIK OCH TEKNOLOGIER  -- Materialteknik -- Kompositmaterial och -teknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Materials Engineering -- Composite Science and Engineering (hsv//eng)
NATURVETENSKAP  -- Kemi -- Materialkemi (hsv//swe)
NATURAL SCIENCES  -- Chemical Sciences -- Materials Chemistry (hsv//eng)

Nyckelord

UN microspheres
thermogravimetric analysis
oxidation resistance
α-U N 2 3
Accident tolerant fuel
UN-UO composite 2
UO fuel 2

Publikations- och innehållstyp

art (ämneskategori)
ref (ämneskategori)

Hitta via bibliotek

Till lärosätets databas

Sök utanför SwePub

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Stäng

Kopiera och spara länken för att återkomma till aktuell vy