Effect of thermal aging on microstructure and carbides of SA508/Alloy 52 dissimilar metal weld

Ge, Y. (författare)
Teknologian Tutkimuskeskus (VTT),Technical Research Centre of Finland (VTT)
Que, Zaiqing (författare)
Teknologian Tutkimuskeskus (VTT),Technical Research Centre of Finland (VTT)
Lindgren, Kristina, 1989 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
visa fler...
Hytönen, N. (författare)
Teknologian Tutkimuskeskus (VTT),Technical Research Centre of Finland (VTT)
Thuvander, Mattias, 1968 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
visa färre...
 (creator_code:org_t)
2023
2023
Engelska.
Ingår i: Materials Characterization. - 1044-5803. ; 200
  • Tidskriftsartikel (refereegranskat)
Abstract Ämnesord
Stäng  
  • A narrow-gap SA508/Alloy 52 dissimilar metal weld (DMW) mock-up, fully representative of an actual nuclear component, was investigated in this work. The microstructure and carbides formed in the low alloy steel fusion boundary (FB) and heat affected zone (HAZ) can act as brittle fracture initiators and could influence the brittle fracture behavior. However, the amount of information available in the open literature on the microstructural changes and carbide formation in DMW occurring upon post-weld heat treatment and long-term thermal aging is very limited. The microstructure and carbide type, morphology and size in the carbide precipitation zone (CPZ, up to 1.5 μm from FB), carbon depletion zone (CDZ, up to 40–50 μm from FB) and HAZ (up to 2 mm from FB) of the plant-relevant DMW in post-weld heat-treated and thermally-aged (400 °C for 15,000 h, corresponding to 90 years of operation) conditions were analyzed with analytical electron microscopy, wide-angle X-ray scattering and atom probe tomography. Long-term thermal aging increases the microhardness peak close to the FB, triples the width of the CPZ and coarsens the carbide size in the HAZ (up to a magnitude). There is no evidence of a significant phosphorus segregation to grain boundaries due to thermal aging.

Ämnesord

TEKNIK OCH TEKNOLOGIER  -- Materialteknik -- Bearbetnings-, yt- och fogningsteknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Materials Engineering -- Manufacturing, Surface and Joining Technology (hsv//eng)
TEKNIK OCH TEKNOLOGIER  -- Materialteknik -- Metallurgi och metalliska material (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Materials Engineering -- Metallurgy and Metallic Materials (hsv//eng)
TEKNIK OCH TEKNOLOGIER  -- Kemiteknik -- Korrosionsteknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Chemical Engineering -- Corrosion Engineering (hsv//eng)

Nyckelord

Carbides
Dissimilar metal welds
Thermal aging
Narrow gap
Alloy 52

Publikations- och innehållstyp

art (ämneskategori)
ref (ämneskategori)

Hitta via bibliotek

Till lärosätets databas

Sök utanför SwePub

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Stäng

Kopiera och spara länken för att återkomma till aktuell vy