SwePub
Sök i LIBRIS databas

  Utökad sökning

id:"swepub:oai:DiVA.org:kth-23362"
 

Sökning: id:"swepub:oai:DiVA.org:kth-23362" > Model films of cell...

LIBRIS Formathandbok  (Information om MARC21)
FältnamnIndikatorerMetadata
00004175naa a2200625 4500
001oai:DiVA.org:kth-23362
003SwePub
008100810s2004 | |||||||||||000 ||eng|
009oai:DiVA.org:miun-3247
024a https://urn.kb.se/resolve?urn=urn:nbn:se:kth:diva-233622 URI
024a https://doi.org/10.1023/B:CELL.0000025403.23775.752 DOI
024a https://urn.kb.se/resolve?urn=urn:nbn:se:miun:diva-32472 URI
040 a (SwePub)kthd (SwePub)miun
041 a engb eng
042 9 SwePub
072 7a ref2 swepub-contenttype
072 7a art2 swepub-publicationtype
100a Fält, Susannau Mittuniversitetet,Institutionen för naturvetenskap (-2008)4 aut0 (Swepub:miun)exsusfal
2451 0a Model films of cellulose II - improved preparation method and characterization of the cellulose film
264 1c 2004
338 a print2 rdacarrier
500 a QC 20100525 QC 20111027
520 a An optimization study of the preparation of spin-coated cellulose model films from the NMMO/DMSO system on silicon wafers has been made. The study shows that the cellulose concentration in the solution determines the cellulose film thickness and that the temperature of the solution affects the surface roughness. A lower solution temperature results in a lower surface roughness at cellulose concentrations below 0.8%. Using the described method, it is possible to prepare films with thicknesses of 30-90 nm with a constant surface roughness by changing the cellulose concentration, i.e. by dilution with DMSO. On these films, water has a contact angle less than 20degrees and about 50% of the material can, according to CP/MAS C-13-NMR spectroscopy on corresponding fibrous material, be considered to consist of crystalline cellulose II type material. It has further been shown that AFM can be used to determine the thickness of cellulose films, in both dry and wet states. In this method, the difference in height between the top surface and the underlying wafer has been measured at an incision made into the cellulose film. The cellulose films have also been spin-coated with the same technique as on the silicon oxide wafer onto the crystal in a quartz crystal microbalance (QCM). These model films were found to be suitable for swelling measurements with the QCM. The films were very stable during this type of measurement and films with different amounts of charges gave different swelling responses depending on their charges. As expected, films with a higher charge showed a higher swelling.
650 7a TEKNIK OCH TEKNOLOGIERx Materialteknik0 (SwePub)2052 hsv//swe
650 7a ENGINEERING AND TECHNOLOGYx Materials Engineering0 (SwePub)2052 hsv//eng
650 7a TEKNIK OCH TEKNOLOGIERx Materialteknikx Pappers-, massa- och fiberteknik0 (SwePub)205032 hsv//swe
650 7a ENGINEERING AND TECHNOLOGYx Materials Engineeringx Paper, Pulp and Fiber Technology0 (SwePub)205032 hsv//eng
653 a AFM
653 a coating
653 a contact angle
653 a dissolving pulp
653 a microbalance
653 a microscopy
653 a NMR
653 a spectroscopy
653 a spinning
653 a surfaces
653 a swelling
653 a quartz-crystal microbalance
653 a n-oxide-monohydrate
653 a light-scattering
653 a adsorption
653 a frequency
653 a chloride
653 a kinetics
653 a setup
653 a Cellulose and paper engineering
700a Wågberg, Larsu KTH,Fiber- och polymerteknologi4 aut0 (Swepub:kth)u14jbte3
700a Vesterlind, Eva-Lottau Mittuniversitetet,Institutionen för naturvetenskap (-2008),FSCN – Fibre Science and Communication Network4 aut0 (Swepub:miun)evaves
700a Larsson, Per Tomas4 aut
710a Mittuniversitetetb Institutionen för naturvetenskap (-2008)4 org
773t Celluloseg 11:2, s. 151-162q 11:2<151-162x 0969-0239x 1572-882X
8564 8u https://urn.kb.se/resolve?urn=urn:nbn:se:kth:diva-23362
8564 8u https://doi.org/10.1023/B:CELL.0000025403.23775.75
8564 8u https://urn.kb.se/resolve?urn=urn:nbn:se:miun:diva-3247

Hitta via bibliotek

  • Cellulose (Sök värdpublikationen i LIBRIS)

Till lärosätets databas

Sök utanför SwePub

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Stäng

Kopiera och spara länken för att återkomma till aktuell vy