Sökning: WFRF:(Odnevall Inger) >
Importance of the m...
Importance of the micro-lattice structure of selective laser melting processed Mo/Mo(x)S(x+1) composite : Corrosion studies on the electrochemical performance in aqueous solutions
-
- Alinejadian, Navid (författare)
- KTH,Yt- och korrosionsvetenskap,Tallinn Univ Technol, Dept Mech & Ind Engn, Ehitajate Tee 5, EE-19086 Tallinn, Estonia.
-
- Kazemi, S. H. (författare)
- Inst Adv Studies Basic Sci, Dept Chem, Zanjan 4513766731, Iran.
-
- Grossberg-Kuusk, M. (författare)
- Tallinn Univ Technol, Dept Mat & Environm Technol, Ehitajate Tee 5, EE-19086 Tallinn, Estonia.
-
visa fler...
-
Kollo, L. (författare)
-
- Odnevall, Inger, 1965- (författare)
- Karolinska Institutet,KTH,Yt- och korrosionsvetenskap,Karolinska Inst, AIMES Ctr Advancement Integrated Med & Engn Sci, Stockholm, Sweden.;KTH Royal Inst Technol, Stockholm, Sweden.;Karolinska Inst, Dept Neurosci, SE-17177 Stockholm, Sweden.
-
- Prashanth, K. G. (författare)
- Tallinn Univ Technol, Dept Mech & Ind Engn, Ehitajate Tee 5, EE-19086 Tallinn, Estonia.;Austrian Acad Sci, Erich Schmid Inst Mat Sci, Jahnstr 12, A-8700 Leoben, Austria.;Vellore Inst Technol, Sch Mech Engn, CBCMT, Vellore 632014, India.
-
visa färre...
-
(creator_code:org_t)
- Elsevier BV, 2022
- 2022
- Engelska.
-
Ingår i: Materials Today Chemistry. - : Elsevier BV. - 2468-5194. ; 26
- Relaterad länk:
-
https://doi.org/10.1...
-
visa fler...
-
https://urn.kb.se/re...
-
https://doi.org/10.1...
-
http://kipublication...
-
visa färre...
Abstract
Ämnesord
Stäng
- Selective laser melting (SLM) based processing of Mo-based samples is challenging due to solidification cracking. We here demonstrate that the addition of 2 wt% MoS2 to the Mo feedstock markedly improves crack mitigation of SLM-processed Mo/MoS2/Mo2S3 composite micro-lattice structures (SLM-Mo/ Mo(x)S(x+1)). Crack inhibition is suggested to be a result of Mo2S3 formation, decreased lattice strain (0.04 4%), and a decrease in accumulated residual stresses. The increased values of polarization resistance from 42.3 and 19.2 kU cm2 to 437 and 78.2 kU cm2, respectively verified the hindering effect of the composition on stress corrosion cracking (SCC) and surface oxidation cracking. However, an increased corrosion current density, from 1.22 to 10.2 mA/cm2, and cathodic Tafel constant, from 175 to 260.5 mV, confirmed the decreased polarization resistance and occurrence of different types of corrosion such as SCC and pitting. The strategy to add 2 wt% MoS2 to the Mo feedstock enables the fabrication of hightemperature micro-lattice structure components with improved corrosion resistance properties applicable in e.g., electronic, power semiconductor heat sinks, offshore-, aerospace-, defense-, or particularly novel sodium-ion energy storage applications.
Ämnesord
- TEKNIK OCH TEKNOLOGIER -- Kemiteknik -- Korrosionsteknik (hsv//swe)
- ENGINEERING AND TECHNOLOGY -- Chemical Engineering -- Corrosion Engineering (hsv//eng)
- TEKNIK OCH TEKNOLOGIER -- Materialteknik -- Kompositmaterial och -teknik (hsv//swe)
- ENGINEERING AND TECHNOLOGY -- Materials Engineering -- Composite Science and Engineering (hsv//eng)
Nyckelord
- Additive manufacturing
- SLM
- Molybdenum
- MoS2
- Novel composite
- Corrosion resistivity