Relaxor behavior and electrothermal properties of Sn- And Nb-modified (Ba,Ca)TiO3 Pb-free ferroelectric

Venkateshwarlu, Sarangi (författare)
City University of Hong Kong
Nayak, Sanjib (författare)
City University of Hong Kong
Marlton, Frederick P. (författare)
Aarhus University
visa fler...
Weyland, Florian (författare)
Technical University of Darmstadt
Novak, Nikola (författare)
Jožef Stefan Institute
Maurya, Deepam (författare)
Virginia Polytechnic Institute and State University
Veerabhadraiah, Yashaswini (författare)
City University of Hong Kong
Borkiewicz, Olaf (författare)
Argonne National Laboratory
Beyer, Kevin A. (författare)
Argonne National Laboratory
Jørgensen, Mads R.V. (författare)
Lund University,Lunds universitet,MAX IV-laboratoriet,MAX IV Laboratory,Aarhus University
Pramanick, Abhijit (författare)
City University of Hong Kong
visa färre...
 (creator_code:org_t)
2020-02-10
2020
Engelska 11 s.
Ingår i: Journal of Materials Research. - : Springer Science and Business Media LLC. - 0884-2914 .- 2044-5326. ; 35:8, s. 1017-1027
  • Forskningsöversikt (refereegranskat)
Abstract Ämnesord
Stäng  
  • Relaxor ferroelectrics have drawn attention for possible applications in solid-state cooling and thermal energy harvesting, owing to their electrothermal energy conversion properties. Here, we have synthesized and characterized the structure-property correlations of a new Sn- and Nb-doped (Ba,Ca)TiO3 relaxor ferroelectric with large pyroelectric and electrocaloric effects over a broad temperature range. We observed two peaks for the temperature-dependent pyroelectric coefficient: (i) -(δP/δT) ∼ 563 μC/(m2 K) at T ∼ 270 K and (ii) -(δP/δT) ∼ 1021 μC/(m2 K) at T ∼ 320 K. In addition, a broad peak for electrocaloric temperature change is observed near 320 K with a relative cooling power of 1/417 J/kg. These properties could be correlated to structural changes observed using X-ray diffraction at two different temperature ranges in the material. Analysis of high-energy X-ray scattering and specific heat capacity data revealed a transition from the cubic to tetragonal phase near Tm ∼ 320 K, whereas an additional increase in the tetragonality (c/a) of the polar phase is observed below Ts ∼ 270 K.

Ämnesord

NATURVETENSKAP  -- Kemi -- Materialkemi (hsv//swe)
NATURAL SCIENCES  -- Chemical Sciences -- Materials Chemistry (hsv//eng)

Nyckelord

electrical properties
ferroelectric
X-ray diffraction

Publikations- och innehållstyp

for (ämneskategori)
ref (ämneskategori)

Hitta via bibliotek

Till lärosätets databas

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Stäng

Kopiera och spara länken för att återkomma till aktuell vy