Development of fibre properties in mill scale high- And low consistency refining of thermomechanical pulp (Part 1)

Ferritsius, Rita (författare)
Mittuniversitetet,Institutionen för kemiteknik,Stora Enso Paper Kvarnsveden Mill, Borlänge
Sandberg, Christer, 1962- (författare)
Mittuniversitetet,Institutionen för kemiteknik,Holmen Paper, Norrköping
Ferritsius, Olof (författare)
Mittuniversitetet,Institutionen för kemiteknik
visa fler...
Rundlöf, Mats (författare)
Capisco, Sweden
Daniel, Geoffrey (författare)
Swedish University of Agricultural Sciences,Sveriges lantbruksuniversitet,Skogens biomaterial och teknologi,Department of Forest Biomaterials and Technology
Mörseburg, Kathrin (författare)
RISE,Material- och ytdesign
Fernando, Dinesh (författare)
Swedish University of Agricultural Sciences,Sveriges lantbruksuniversitet,Skogens biomaterial och teknologi,Department of Forest Biomaterials and Technology
visa färre...
 (creator_code:org_t)
 
2020-09-16
2020
Engelska.
Ingår i: Nordic Pulp & Paper Research Journal. - : De Gruyter Open Ltd. - 0283-2631 .- 2000-0669. ; 35:4, s. 589-599
  • Tidskriftsartikel (refereegranskat)
Abstract Ämnesord
Stäng  
  • The aim of this study was to evaluate changes in fibre properties with high (HC)- and low consistency (LC) refining of TMP and determine how these contribute to tensile index. Two process configurations, one with only HC refining and another with HC refining followed by LC refining were evaluated in three TMP mainline processes in two mills using Norway spruce. An increase in tensile index for a given applied specific energy was similar for all LC refiners in the three lines, despite differences in the fibre property profiles of the feed pulps. Compared with only HC refined pulps at a given tensile index, HC+LC refined pulps had greater fibre wall thickness, similar fibre length, strain at break and freeness, but lower light scattering coefficient, fibre curl and external fibrillation. The degree of internal fibrillation, determined by Simons' stain measurements, was similar for both configurations at a given tensile index. The results indicate that the increase in tensile index in LC refining is largely influenced by a decrease in fibre curl and in HC refining by peeling of the fibre walls. Compared at a given tensile index, the shive content (Somerville mass fraction) was similar for both HC+LC and HC refining.

Ämnesord

TEKNIK OCH TEKNOLOGIER  -- Materialteknik -- Pappers-, massa- och fiberteknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Materials Engineering -- Paper, Pulp and Fiber Technology (hsv//eng)

Nyckelord

fibre properties
high consistency refining
low consistency refining
specific energy
TMP
Light scattering
Refining
Textile fibers
Thermomechanical pulp
Thermomechanical pulping process
Fibre wall thickness
Light scattering coefficient S
Low consistency
Norway spruce
Process configuration
Strain at break
Pulp refining

Publikations- och innehållstyp

ref (ämneskategori)
art (ämneskategori)

Hitta via bibliotek

Till lärosätets databas

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Stäng

Kopiera och spara länken för att återkomma till aktuell vy