Formation process and superparamagnetic properties of (Mn,Ga)As nanocrystals in GaAs fabricated by annealing of (Ga,Mn)As layers with low Mn content

Sadowski, Janusz (författare)
Lund University,Lunds universitet,MAX IV-laboratoriet,MAX IV Laboratory
Domagala, Jaroslaw Z (författare)
Institute of Physics, Polish Academy of Sciences, Warszawa, Polen
Mathieu, Roland (författare)
Uppsala universitet,Fasta tillståndets fysik
visa fler...
Kovács, András (författare)
Center for Electron Nanoscopy, Technical University of Denmark, Kongens Lyngby, Danmark, and, Ernst Ruska-Centre and Peter Grünberg Institute, Research Centre Jülich, Tyskland
Kasama, Takeshi (författare)
Center for Electron Nanoscopy, Technical University of Denmark, Kongens Lyngby, Danmark
Dunin-Borkowski, Rafael E (författare)
Center for Electron Nanoscopy, Technical University of Denmark, Kongens Lyngby, Danmark, and, Ernst Ruska-Centre and Peter Grünberg Institute, Research Centre Jülich, Tyskland
Dietl, Tomasz (författare)
MAX-IV Laboratory, Lund University, and, Faculty of Physics, University of Warsaw, Polen
visa färre...
 (creator_code:org_t)
2011
2011
Engelska.
Ingår i: Physical Review B. Condensed Matter and Materials Physics. - 1098-0121 .- 1550-235X. ; 84:24, s. 245306-
  • Tidskriftsartikel (refereegranskat)
Abstract Ämnesord
Stäng  
  • X-ray diffraction, transmission electron microscopy, and magnetization measurements are employed to study the structural and magnetic properties of Mn-rich (Mn,Ga)As nanocrystals embedded in GaAs. These nanocomposites are obtained by moderate-temperature (400 degrees C) and high-temperature (560 degrees C and 630 degrees C) annealing of (Ga,Mn)As layers with Mn concentrations between 0.1% and 2%, grown by molecular beam epitaxy at 270 degrees C. Decomposition of (Ga,Mn)As is already observed at the lowest annealing temperature of 400 degrees C for layers with initial Mn content of 1% and 2%. Both cubic and hexagonal (Mn, Ga) As nanocrystals, with similar diameters of 7-10 nm, are observed to coexist in layers with an initial Mn content of 0.5% and 2% after higher-temperature annealing. Measurements of magnetization relaxation in the time span 0.1-10 000 s provide evidence for superparamagnetic properties of the (Mn,Ga)As nanocrystals, as well as for the absence of spin-glass dynamics. These findings point to weak coupling between nanocrystals even in layers with the highest nanocrystal density.

Ämnesord

NATURVETENSKAP  -- Fysik -- Den kondenserade materiens fysik (hsv//swe)
NATURAL SCIENCES  -- Physical Sciences -- Condensed Matter Physics (hsv//eng)
NATURVETENSKAP  -- Fysik (hsv//swe)
NATURAL SCIENCES  -- Physical Sciences (hsv//eng)

Nyckelord

TECHNOLOGY
TEKNIKVETENSKAP
Teknisk fysik med inriktning mot fasta tillståndets fysik
Engineering Science with specialization in Solid State Physics
molecular beam epitaxy
nanomagnetism
magnetic semiconductors

Publikations- och innehållstyp

ref (ämneskategori)
art (ämneskategori)

Hitta via bibliotek

Till lärosätets databas

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Stäng

Kopiera och spara länken för att återkomma till aktuell vy