Combined in Situ Quartz Crystal Microbalance with Dissipation Monitoring, Indirect Nanoplasmonic Sensing, and Vibrational Sum Frequency Spectroscopic Monitoring of Alkanethiol-Protected Copper Corrosion

Schwind, Markus, 1983 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
Hosseinpour, Saman (författare)
KTH,Yt- och korrosionsvetenskap,Kungliga Tekniska Högskolan (KTH),Royal Institute of Technology (KTH)
Johnson, C. Magnus (författare)
KTH,Yt- och korrosionsvetenskap,Kungliga Tekniska Högskolan (KTH),Royal Institute of Technology (KTH)
visa fler...
Langhammer, Christoph, 1978 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
Zoric, Igor, 1946 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
Leygraf, Christofer (författare)
KTH,Yt- och korrosionsvetenskap,Kungliga Tekniska Högskolan (KTH),Royal Institute of Technology (KTH)
Kasemo, Bengt Herbert, 1942 (författare)
Chalmers tekniska högskola,Chalmers University of Technology
visa färre...
 (creator_code:org_t)
2013-05-28
2013
Engelska.
Ingår i: Langmuir. - : American Chemical Society (ACS). - 0743-7463 .- 1520-5827. ; 29:23, s. 7151-7161
  • Tidskriftsartikel (refereegranskat)
Abstract Ämnesord
Stäng  
  • In this study, we have applied three techniques to simultaneously and in situ study the initial stage of corrosion of copper protected by a self-assembled monolayer of octadecanethiol (ODT). We combined quartz crystal microbalance with dissipation monitoring (QCM-D), indirect nanoplasmonic sensing (INPS), and vibrational sum frequency spectroscopy (VSFS) and obtained complementary information about mass uptake and optical and spectroscopic changes taking place during the initial corrosion phase. All three techniques are very sensitive to the formation of a corrosion film (thickness in the range 0-0.41 nm) under mildly corrosive conditions (dry air, <0.5% relative humidity). The three techniques yield information about the viscoelasticity of the corrosion film (QCM-D), the homogeneity of the corrosion reaction on the surface (INPS), and the stability of the ODT. protection layer (VSFS). Furthermore, by also studying the corrosion process in humid air (ca. 70% relative humidity), we illustrate how the combination of these techniques can be used to differentiate between simultaneously occurring processes, such as water adsorption and corrosion product formation.

Ämnesord

NATURVETENSKAP  -- Kemi -- Annan kemi (hsv//swe)
NATURAL SCIENCES  -- Chemical Sciences -- Other Chemistry Topics (hsv//eng)
TEKNIK OCH TEKNOLOGIER  -- Annan teknik (hsv//swe)
ENGINEERING AND TECHNOLOGY  -- Other Engineering and Technologies (hsv//eng)

Nyckelord

Corrosion products
Corrosion reaction
Corrosive conditions
Quartz crystal microbalance with dissipation monitoring
Situ quartz crystal microbalance
Spectroscopic changes
Spectroscopic monitoring
Vibrational sum-frequency spectroscopies

Publikations- och innehållstyp

ref (ämneskategori)
art (ämneskategori)

Hitta via bibliotek

  • Langmuir (Sök värdpublikationen i LIBRIS)

Till lärosätets databas

Kungliga biblioteket hanterar dina personuppgifter i enlighet med EU:s dataskyddsförordning (2018), GDPR. Läs mer om hur det funkar här.
Så här hanterar KB dina uppgifter vid användning av denna tjänst.

 
pil uppåt Stäng

Kopiera och spara länken för att återkomma till aktuell vy